Cheaptubes.com is The Source for OH Functionalized Nanotubes-OH CNTs

CheapTubes.com is "The Source for OH functionalized Nanotubes!

Our OH Functionalized Nanotubes are available with Hydroxyl (OH) functional groups bonded to the ends and sidewalls of the CNTs. Please note - OH functionalized nanotubes have primarily OH functional groups whereas the COOH functionalized nanotubes have mostly COOH groups with a small concentration of OH groups as well.


OH Functionalized Nanotubes

 

 

OH Functionalized Carbon Nanotubes Prices

 

OH Functionalized Single Walled Nanotubes 1-2nm

OH Functionalized Multi Walled Nanotubes <8nm

OH Functionalized Multi Walled Nanotubes 8-15nm

OH Functionalized Multi Walled Nanotubes 10-20nm

OH Functionalized Multi Walled Nanotubes 20-30nm

OH Functionalized Multi Walled Nanotubes 30-50nm

OH Functionalized Multi Walled Nanotubes >50nm

 

OH Functionalized Nanotubes-OH-CNTs Manufacturing Method:CCVD

 

     Our OH Functionalized Nanotubes-OH MWNTs 20-30nm & OH Functionalized Nanotubes -OH MWNTs 20-40nm products have merged into one product the OH Functionalized Nanotubes-OH MWNTs 20-30nm.  There were process refinements that lead to all of them being classified as 20-30nm.  The two products were previously manufactured in the same production run so this change should have little impact on the products performance.

 

OH Functionalized Nanotubes-OH-SWNT 90s Specifications

OH functionalized Nanotubes-OH-SWNTs90s TEM pic

A TEM image of our OH Functionalized Nanotubes-OH-SWNTs 90wt% 1-2nm OD

Outer Diameter: 1-2nm

Inside Diameter: 0.8-1.6nm

Ash: <1.5 wt%

Purity: >90 wt%

Additional MWNT content: >5wt%

Amorphous Carbon Content: <3wt%

Length: 5-30um

Specific Surface Area: 407 m2/g

Electrical Conductivity: >100 S/cm

OH-SWNTs contain 3.9% OH groups

Bulk density: 0.14 g/cm3

True density: ~2.1 g/cm3

OH Functionalized Nanotubes-OH-MWNTs-8nm Specifications

OH Functionalized Nanotubes-OH-MWNTs_<8nm od

A TEM image of our OH Functionalized Nanotubes-OH-MWNTs 95wt% <8nm OD

Outer Diameter: <8nm

Inside Diameter: 2-5nm

Ash: <1.5 wt%

Purity: >95 wt%

Length: 10-30um

Electrical Conductivity: >100 S/cm

Bulk density: 0.27 g/cm3

True density: ~2.1 g/cm3

Specific Surface Area: 500 m2/g

OH-MWNTs contain 5.5% OH groups

OH Functionalized Nanotubes-OH-MWNTs 8-15nm Specifications

OH Functionalized Nanotubes-OH-MWNTs_8-15nm od

A TEM image of our OH Functionalized Nanotubes OH-MWNTs 95wt% 8-15nm OD

Outer Diameter: 8-15nm

Inside Diameter: 3-5nm

Ash: <1.5 wt%

Purity: >95 wt%

Length: 10-50um

Specific Surface Area: 233 m2/g

Electrical Conductivity: >100 S/cm

Bulk density: 0.15 g/cm3

True density: ~2.1 g/cm3

OH-MWNTs contain 3.7% OH groups

OH Functionalized Nanotubes-OH-MWNTs 10-20nm Specifications

OH Functionalized Nanotubes-OH-MWNTs 10-20nm_od

A TEM Image of our OH Functionalized Nanotubes-OH-MWNTS 95wt% 10-20nm OD

Outer Diameter: 10-20nm

Inside Diameter: 3-5nm

Ash: <1.5 wt%

Purity: >95 wt%

Length: 10-30um

Specific Surface Area: 233 m2/g

Electrical Conductivity: >100 S/cm

Bulk density: 0.22 g/cm3

True density: ~2.1 g/cm3

OH-MWNTs contain 2.0% OH groups

OH Functionalized Nanotubes-OH-MWNTs 20-30nm Specifications

OH functionalized nanotubes-OH-MWNTs 95s 20-30nm od TEM pic

A TEM image of our OH Functionalized Nanotubes OH-MWNTs 95wt% 20-30nm OD

Outer Diameter: 20-30nm

Inside Diameter: 5-10nm

Ash: <1.5 wt%

Purity: >95 wt%

Length: 10-30um

Specific Surface Area: 110 m2/g

Electrical Conductivity: >100 S/cm

Bulk density: 0.28 g/cm3

True density: ~2.1 g/cm3

OH-MWNTs contain 1.6% OH groups

OH Functionalized Nanotubes-OH-MWNTs 30-50nm Specifications

OH functionalized Nanotubes-OH-MWNTs 95s 30-50nm od TEM pic

A TEM image of our OH Functionalized Nanotubes-OH MWNTs 95wt% 30-50nm OD

Outer Diameter: 30-50nm

Inside Diameter: 5-10nm

Ash: <1.5 wt%

Purity: >95 wt%

Length: 10-20um

Specific Surface Area: 60 m2/g

Electrical Conductivity: >100 S/cm

Bulk density: 0.28 g/cm3

True density: ~2.1 g/cm3

OH-MWNTs contain 1.0% OH groups

OH Functionalized Nanotubes-OH-MWNTs 50nm Specifications

OH functionalized nanotubes-OH-MWNTs 95s >50nm od TEM pic

A TEM image of our OH Functionalized Nanotubes OH-MWNTs 95wt% >50nm OD

Outer Diameter: 50-80nm

Inside Diameter: 5-10nm

Ash: <1.5 wt%

Purity: >95 wt%

Length: 10-20um

Specific Surface Area: 60 m2/g

Electrical Conductivity: >100 S/cm

Bulk density: 0.18 g/cm3

True density: ~2.1 g/cm3

OH-MWNTs contain 0.7% OH groups


       Our OH Functionalized Nanotubes-OH CNTs are produced by Catalyzed Chemical Vapor Deposition. To help us better assist you, please select either the OH or the COOH when placing an order.

 OH Functionalized Nanotubes-OH-CNTs Key Benefits

  • CCVD Fabrication means high purity, low cost
  • Available in metric ton quantities
  • Suitable for a wide variety of applications


OH Functionalized Nanotubes Prices- OH-CNTs-Prices

 

OH Functionalized Nanotubes OH-CNTs

SKU #

OH Functionalized Nanotubes Prices -OH-CNTs Prices (in Grams and Kilograms)

  1 g      10 g      25 g       50 g      100 g      500 g    1KG   

OH Functionalized Nanotubes OH-SWNTs 90wt% 1-2nm OD

 

sku-0102

150

1,350

2,750

5,000

9,500

42,500

80,000

OH Functionalized Nanotubes OH- MWNTs 95wt% <8nm OD

sku-030201

40

250

350

650

1,200

3,000

4,000

OH Functionalized Nanotubes OH MWNTs 95wt% 8-15nm OD

sku-030202

25

150

275

500

900

2,750

3,750

OH Functionalized Nanotubes OH MWNTs 95wt% 10-20nm OD

 

sku-030203

25

150

275

500

900

2,750

3,600

OH Functionalized Nanotubes OH MWNTs 95wt% 20-30nm OD

sku-030204

15

125

250

450

800

1,250

1,750

OH Functionalized Nanotubes OH MWNTs 95wt% 30-50nm OD

sku-030206

15

125

250

450

800

1,150

1,500

OH Functionalized Nanotubes OH MWNTs 95wt% >50nm OD

sku-030207

15

125

250

450

800

1,150

1,500

Valid XHTML 1.0 Transitional Valid CSS!